ASTM-B-209

Physical Properties
  • Minimum Tensile Strength - 20,000 psi
  • Maximum Tensile Strength - 26,000 psi
  • Minimum Yield Strength - 17,000 psi
  • Elongation (0.009 to 0.012" Thick) - 1%
  • Elongation (0.013 to 0.019" Thick) - 2%
  • Elongation (0.020 to 0.031" Thick) - 3%
Unit of Measure

Specifications

Width

12 in

Length

18 in

Alloy

3003 Aluminum Alloy

Thickness

0.0120 in

Thickness Tolerance

0.0008 in

American Society for Testing and Materials (ASTM) Steel Standard

ASTM-B-209

Material Form

Sheet

Temper

H14 Half Hard Temper

Chemical Composition

Maximum Silicon Composition

0.60 %

Maximum Iron Composition

0.70 %

Maximum Copper Composition

0.20 %

Maximum Manganese Composition

1.50 %

Maximum Zinc Composition

0.10 %

Maximum Others Composition (Each)

0.05 %

Maximum Others Composition (Total)

0.15 %

Chemical Composition Table



Physical Properties

Minimum Tensile Strength

20,000 psi

Maximum Tensile Strength

26,000 psi

Minimum Yield Strength

17,000 psi

Minimum Elongation (0.009 to 0.012 Inch (in) Thick)

1 %

Minimum Elongation (0.013 to 0.019 Inch (in) Thick)

2 %

Minimum Elongation (0.020 to 0.031 Inch (in) Thick)

3 %